Ziro 3D PLA Pro Filament 1.75mm 1kg Lavender 3d printers accessory
- Lavender
- Filament
Vi tar imot kryptovaluta — slik kan kryptovalutaene du eier, kjøpe ekte maskinvare.Betal med krypto, bruk den på ekte maskinvare. Gratis, forsikret levering verden over for bestillinger over 399 $. Nøytrale kartonger uten merking, sendt fra Tyskland.Gratis, forsikret levering over 399 $. Kursen din er låst i 30 minutter når kassen åpnes.Kurs låst i 30 minutter. Alle varer er forseglet, serienummerkontrollert og dekket av 24 måneders garanti.Forseglet, 24 måneders garanti.
Taulman 3D
PETG filament for functional parts prints at 235–242 °C on a bed up to 68 °C, 2.85 mm diameter, 1 kg spool, 5900 PSI tensile strength
Taulman 3D TECH-G is a PETG polymer filament designed for functional prototyping and end-use parts. The material offers a tensile strength of 5900 PSI and 3% elongation, providing durability for mechanical testing. It comes in a 1kg spool with a 2.85 mm diameter in black.
Switch to TECH-G when parts must withstand higher mechanical stress or repeated assembly cycles. The increased tensile strength and controlled elongation reduce brittle failure in functional brackets, jigs and enclosures. The print temperature range of 235C to 242C works on most all-metal hotends without specialised hardware.
The filament prints on a heated bed up to 68C and adheres well to common surfaces such as PEI or glass with glue stick. The 2.85 mm diameter suits Bowden and direct-drive extruders calibrated for 3 mm class filament. Low warping characteristics free up design freedom for larger flat components without an enclosed chamber.
| Brand | taulman3d |
|---|---|
| Color | Black |
| Type | Filament |
The spool is 2.85 mm diameter filament, so the printer must accept 2.85 mm (often called 3 mm class) material and have a compatible drive gear and Bowden tube or direct-drive path.
Heat the bed to 68 °C maximum; higher temperatures are not recommended and can cause adhesion issues or warping on this PETG formulation.
If prints show popping, stringing or layer adhesion loss, dry the spool at low heat for several hours; replace it once the 1 kg roll is consumed or if the material becomes brittle after repeated moisture cycles.
Også i denne avdelingen
Samme hylle, samme kasse — åtte mynter og 30 minutters kurslås.
Det du betaler med, og det du ser prisene i.
Sendes fra lommeboken din i kassen
Kun visning — katalogen er prissatt i USD
Fant ingen valuta.
Velg språket nettstedet snakker til deg på.
Ingen språk samsvarer.
Ny her?
Har du allerede en konto?
Det finnes ingen automatisk tilbakestilling: butikken sender ikke e-post, så det finnes ingen engangslenke å be om. La adressen stå på kontoen, så blir den behandlet manuelt.
Forespørsel registrert
Ingenting er på vei til innboksen din — butikken sender ingen e-post i det hele tatt. Noen behandler dette manuelt.
Husket du det likevel?